• ISSN [ Online ] : 3139-1141

Volume 1 - Issue 5, November - December 2026

  • Home
  • November - December 2026

Decoupling the Synergistic Effects of Ball Milling Duration and Alkali Concentration on the Strength Development of GGBS Based Alkali Activated Concrete


📑 Paper Information
📑 Paper Title Decoupling the Synergistic Effects of Ball Milling Duration and Alkali Concentration on the Strength Development of GGBS Based Alkali Activated Concrete
👤 Authors Rahul Tripathi, Sharad Kumar Soni, Kapil Kumar Soni
📘 Published Issue Volume 1 Issue 5
📅 Year of Publication 2026
🆔 Unique Identification Number IJARSMET-V1I5P28
📑 Search on Google Click Here
📝 Abstract
The strength development of ground granulated blastfurnace slag (GGBS)based alkaliactivated concrete (AAC) is governed by two activation routes that are usually optimised in isolation: mechanical activation through ball milling and chemical activation through alkali concentration. This study presents a systematic experimental investigation into the coupled effects of ball milling duration and NaOH molarity on the fresh and mechanical properties of GGBSbased AAC. A total of 30 mixes were prepared using a full factorial design, comprising six milling durations (0, 2, 4, 6, 8, and 10 h) and five NaOH molarities (4, 6, 8, 10, and 12 M). Fresh properties were evaluated through slump, setting time, and fresh density. Mechanical properties including compressive strength (7 and 28 days), split tensile strength, flexural strength, and modulus of elasticity (28 days) were determined according to IS and ASTM standards. Results demonstrate that both milling duration and molarity influence performance nonmonotonically, and that their interaction is statistically significant. Unmilled GGBS attained its highest 28day compressive strength at 10 M NaOH, whereas intermediate milling of 4–6 h shifted the strength maximum to approximately 8 M. The optimum combination was 6 h milling with 8 M NaOH, achieving a 28day compressive strength of 79.5 MPa, a 15.9% increase over the unmilled 10 M reference mix. Overmilling beyond 6 h reduced strength across all molarities, most notably at 12 M. Split tensile, flexural, and elastic modulus improvements of 22.4%, 23.7%, and 19.4%, respectively, were recorded for the optimum mix. The enhancements are attributed to mechanochemically induced amorphisation, increased surface reactivity, and improved gel densification. The results provide practical guidance for reducing alkali dosage in GGBSbased AAC through controlled mechanical pretreatment.
📝 How to Cite
Rahul Tripathi, Sharad Kumar Soni, Kapil Kumar Soni, "Decoupling the Synergistic Effects of Ball Milling Duration and Alkali Concentration on the Strength Development of GGBS Based Alkali Activated Concrete" International Journal of Advance Research in Science, Management, Engineering and Technology, V1(5): Page(195-200) November - December 2026. ISSN: 3139-1141. www.ijarsmet.com. Published by Scientific and Academic Research Publishing.